Dedicated to New Material Development
1, Saturation Magnetic Induction BS [T]: ~ 1.2 T
2, Coercivity (static, 50Hz) HC [A/m]: < 3 A/m
3, Saturation Point λs [ppm]: < 0.05 ppm
4 , Resistivity ρel [µΩm]: ~ 1.15 µΩm
5, Curie Temperature TC [°C]: ~ 600 °C
6, Operating Temperature Tw [°C]: -40 ~ +200 °C
Temperature VS δμ (F=10K)
Frequency VS permeability
Compare of magnetic flux density
Annealing without magnetic field
Annealing with transverse magnetic field
Annealing with vertical magnetic field
Core loss vs frequency
Magnetic flux density vs Core loss(F=100K)
Permeability vs Frequency